# AzureFilm PC-ABS print settings (nozzle, bed, dry)

AzureFilm PC-ABS prints at 270 °C (518 °F) nozzle and 110 °C (230 °F) bed, per Open Filament Database.

Print at 270 °C (518 °F) nozzle, 110 °C (230 °F) bed.

Source: Open Filament Database

## Sources & notes

AzureFilm PC-ABS (PC) has a recommended nozzle temperature of 270 °C (518 °F) and a recommended bed temperature of 110 °C (230 °F), according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/azurefilm/materials/PC/filaments/pc_abs/index.json; dataset imported 2026-10-13).

Dataset imported: 2026-10-13. Open Filament Database generation date, not a lab test.

- Material: PC
- Nozzle: 270 °C (518 °F)
- Bed: 110 °C (230 °F)
- Dry: not in our current sources
- Print speed: not in our current sources
- Hardened nozzle: not recorded
- Source: https://api.openfilamentdatabase.org/api/v1/brands/azurefilm/materials/PC/filaments/pc_abs/index.json

## What nozzle temperature does AzureFilm PC-ABS recommend?

AzureFilm PC-ABS lists a recommended nozzle temperature of 270 °C (518 °F).

## What bed temperature does AzureFilm PC-ABS recommend?

AzureFilm PC-ABS lists a recommended bed temperature of 110 °C (230 °F).

## What print speed does AzureFilm PC-ABS list?

Print speed and volumetric flow are not in our current sources in the imported sources.

## Does AzureFilm PC-ABS require an enclosure?

An enclosure requirement is not in our current sources. No chamber temperature is listed either.

## Does AzureFilm PC-ABS require a hardened nozzle?

A hardened-nozzle requirement is not in our current sources.

## How should AzureFilm PC-ABS be dried?

Drying temperature and drying time for AzureFilm PC-ABS are not in our current sources.

## What spool weights does AzureFilm PC-ABS come in?

Listed spool weights: 1 kg (1000 g).

## What is the price per kilogram of AzureFilm PC-ABS?

Price per kilogram is not in our current sources.