# Overture TPU vs SUNLU TPU

Overture TPU. Print at 210–240 °C nozzle, 30–60 °C bed. Dry at 70 °C if it's been open. No drying time on the source.

SUNLU TPU. Print at 210–240 °C nozzle, 30–60 °C bed.

## Sources & notes

Overture TPU lists a recommended nozzle temperature of 210–240 °C and a recommended bed temperature of 30–60 °C, according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/overture/materials/TPU/filaments/tpu/index.json; dataset imported 2026-10-13). SUNLU TPU lists a recommended nozzle temperature of 210–240 °C and a recommended bed temperature of 30–60 °C, according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/sunlu/materials/TPU/filaments/tpu/index.json; dataset imported 2026-10-13). Where a source leaves a value blank, this comparison leaves it blank.

Overture TPU lists 210–240 °C.
SUNLU TPU lists 210–240 °C.
Overture TPU lists 30–60 °C.
SUNLU TPU lists 30–60 °C.